Designation by Standards

Steel No. DIN EN AISI JIS ГОСТ
1.3401 X120Mn12 - A128 grade A / 110G13L


Chemical Composition (in weight %)

C Si Mn Cr Mo Ni V W Others
1.20 0.40 12.50 max. 1.50 - - - - -


Description
Austenitic Mn-steel. The well-known Hadfield steel still has broad applications in the mineral processing industry. Especially under impact loading Hadfield steel displays good wear resistance due to its high cold work ability. However, Hadfield steel is not corrosion resistant.
Applications
Components for dredgers and crushers, conveying machines: crushings jaws, impact wedges, linings, etc.

Physical properties (avarage values) at ambient temperature
Modulus of elasticity [103 x N/mm2]: 190-210
Density [g/cm3]: 7.88

Hardening
Harden from a temperature of 1000-1050oC followed by water quenching. Hardness after quenching is about 200 HB.

Mechnical properties at ambient temperature:
0.2 % proof stress (N/mm2): 350
Tensile strength (N/mm2): 800-1000

Forging
Hot forming temperature: 1050-850oC

Machinability
The machinability of this steel is poor.

Remark
All technical information is for reference only.